Housing material | HT250 High strength cast iron from F37,47,57,67,77,87,F97,127,157,167,187 |
Housing hardness | HBS90-240 |
Gear material | 20CrMnTi |
Surface hardnesss of gear | HRC58°-62° |
Gear core hardness | HRC33°-40° |
Input/Output shaft material | 40CrMnTi |
Input/Output shaft hardness | HBS241°-286° |
Shaft at oil seal postion hardness | HRC48 ° -55 ° |
Machining precision of gears material | Accurate grinding 6-5 grade |
Heat treatment | Tempering, Cementing, Quenching etc |
Efficiency | up to 90% |
Noise(Max) | 50-68dB |
Input Power | 0.18~200kw |
Allowable Torque ( N.m ) | 200~18000 |
Transmission Ratio | 3.81~280.76 |
Unit model | Foot mounted,flange mounted,hollow shaft mounted |
Input method | flange input,inline input,shaft input |
Vibration | ≤ 20um |
Backlash | ≤ 20Arcmin |
Lubricant | VG220 |
Motor | IP55, F class |
Motor shaft | 40Cr, Tempering, cementing,quenching etc. |
Contact Person : | Francis |
---|